top of page

Home  ›  Products  ›  Standard-Specific Test Fixtures  ›  Rebar Stress Corrosion Cracking Fixture GOST 34028

UGC-ST-270 rebar stress corrosion cracking fixture with lever arms, dead weights and transparent test cell by Universal Grip
UGC-ST-270 rebar stress corrosion cracking fixture with lever arms, dead weights and transparent test cell by Universal Grip
UGC-ST-270 Rebar Stress Corrosion Cracking Fixture GOST 34028 by Universal Grip, view 2
Product photo 3
Product photo 4

Rebar Stress Corrosion Cracking Fixture GOST 34028

Free-standing dead-weight rig that holds reinforcing bar under constant tensile load in a 100 °C calcium ammonium nitrate solution.

Brand: Universal Grip  |  Model: UGC-ST-270  |  ● Configured to order

  • Designed for stress corrosion cracking tests on reinforcing steel, such as GOST 34028

  • Lever arms with dead weights hold a constant tensile load on the bar

  • Weight set included: 5 x 1 kg, 5 x 2 kg and 5 x 5 kg (40 kg / 88 lb in total)

  • Transparent test cell holds the calcium ammonium nitrate solution

  • Heated bath maintains the 100 °C (212 °F) test temperature

  • Free-standing frame with leveling feet; no testing machine needed

Standards: GOST 34028

Trusted by Global Companies

Dead-weight stress corrosion cracking rig for reinforcing steel

The UGC-ST-270 is a stress corrosion cracking test fixture for reinforcing rolled products used in reinforced concrete, designed for tests such as GOST 34028. Unlike most fixtures in our range it does not mount in a testing machine. It is a free-standing rig that keeps a bar specimen under constant tensile load in a hot corrosive solution for the whole test, so a long exposure does not tie up a tensile tester. It is used by reinforcing steel producers, labs qualifying prestressing steel, construction materials laboratories and corrosion researchers.

 

How it works

The bar specimen passes through a transparent test cell filled with calcium ammonium nitrate solution at 100 °C (212 °F). Lever arms loaded with dead weights pull on the bar and hold the tensile load constant, with no drive or controller involved. The load stays on until the bar cracks or the test duration ends. A heated bath maintains the test temperature, the transparent cell keeps the specimen and the solution in view, and leveling feet let the frame be set level before the weights go on.

 

Loading and weights

A weight set is included: five 1 kg, five 2 kg and five 5 kg weights, 15 pieces with a combined mass of 40 kg (about 88 lb). The mix of sizes lets the load be built up in small increments. The force that reaches the specimen depends on the lever arms, so the maximum load is given on request and confirmed against your bar diameter range and required test load.

 

What to specify

  • Bar diameter range: the reinforcing bars or rolled products you need to hold.

  • Required test load: the constant tensile load your procedure calls for.

  • Heating unit: whether the heating unit is to be supplied with the rig.

 

Typical applications

  • Reinforcing steel producers

  • Prestressing steel qualification

  • Construction materials laboratories

  • Corrosion research

 

Related equipment

The rig covers the long-duration exposure only. Tensile tests on the same reinforcing steel are run on a testing machine: our Galdabini hydraulic universal testing machines handle high-capacity bar testing, fitted with wedge grips or hydraulic grips. Our metals testing page gives an overview of grips and fixtures for steel products, and the standard-specific fixtures hub lists other single-purpose rigs.

Dimensional drawings and 3D models are available on request. Send us the bar diameter range, the required test load and whether you want the heating unit included, and we will configure the rig: request a quote.

Product video

At a glance

  • Test type: Stress corrosion cracking, constant load

  • Standard: GOST 34028

  • Specimen: Reinforcing bars and rolled products

  • Loading: Lever arms with dead weights

  • Weights included: 5 x 1 kg, 5 x 2 kg, 5 x 5 kg

  • Test medium: Calcium ammonium nitrate solution

Rebar Stress Corrosion Cracking Fixture GOST 34028 Specifications

TEST TYPE

Stress corrosion cracking, constant load

 

STANDARD

GOST 34028

 

SPECIMEN

Reinforcing bars and rolled products

 

LOADING

Lever arms with dead weights

 

WEIGHTS INCLUDED

5 x 1 kg, 5 x 2 kg, 5 x 5 kg

 

TEST MEDIUM

Calcium ammonium nitrate solution

 

TEST TEMPERATURE

100 °C (212 °F)

 

MAX. LOAD

On request

 

PART REF.

UGC-ST-270

 

Models & Options

  • Stress corrosion cracking rig — Free-standing frame with lever arms, transparent test cell and weight set (Specify at order)

  • Heating unit — Keeps the bath at the 100 °C test temperature; state at order whether it is to be supplied (Specify at order)

  • Bar diameter range — Rig matched to the bar diameters you test (On request)

  • Test load — Maximum load confirmed against your required test load (On request)

What's Included

  • Free-standing frame with leveling feet and lever arms

  • Transparent test cell for the test solution

  • Weight set: 5 x 1 kg, 5 x 2 kg and 5 x 5 kg

  • Heating unit: state at order whether it is to be supplied

  • Dimensional drawings and 3D models available on request

Supported Test Standards

  • GOST 34028 — Reinforcing rolled products for reinforced concrete constructions

Compatible Grips & Fixtures

“Customer quote”

Related Equipment

UGC-ST-610 Wire Insulation Notch Resistance Fixture

UGC-ST-610 Wire Insulation Notch Resistance Fixture

Cut-through fixture for notch resistance testing of wire and cable insulation, designed for LV 112 and ASTM D3032 tests;

UGC-ST-300 Fastener Shear Fixture 400 kN

UGC-ST-300 Fastener Shear Fixture 400 kN

Heavy-duty 400 kN shear fixture with interchangeable inserts for threaded fasteners M6 to M24, used between compression

UGC-ST-590 Electrical Varnish Helical Coil Bond Fixture

UGC-ST-590 Electrical Varnish Helical Coil Bond Fixture

Helical coil bond strength fixture for electrical insulating varnishes, designed for ASTM D2519 tests, with roller suppo

UGC-ST-310 Blind Rivet Shear and Tensile Fixture ISO 14589

UGC-ST-310 Blind Rivet Shear and Tensile Fixture ISO 14589

Fixture set for blind rivet shear, tensile, mandrel head retention and mandrel break tests, with inserts for 4.8 mm and

Rebar Stress Corrosion Cracking Fixture GOST 34028 FAQ

Does the UGC-ST-270 need a testing machine?

No. It is a free-standing rig with leveling feet, and the load comes from dead weights on lever arms.

 

How is the load applied and held?

Lever arms loaded with dead weights pull on the bar and hold a constant tensile load. The load stays on until the bar cracks or the test duration ends.

 

Which weights are included?

Five 1 kg, five 2 kg and five 5 kg weights, 40 kg (about 88 lb) in total.

 

What test medium and temperature is it designed for?

A calcium ammonium nitrate solution at 100 °C (212 °F), held in a transparent test cell.

 

Is the heating unit included?

State at order whether the heating unit is to be supplied with the rig. We confirm the scope of supply in the quote.

 

What bar diameters and loads can it handle?

Maximum load is given on request. Send us your bar diameter range and required test load and we will confirm the configuration.

 

Need help configuring a standard-specific test fixture?

Tell us your material, test standard and specimen size. We will recommend the frame, force sensor, grips and fixtures, and send a quote.

bottom of page